EstNickel-Iron, humilis dilatatio mixturae continens 36% Nickel cum libra ferri.Dimensiones fere constantes conservat in temperaturis atmosphaerici normalibus et humilem expansionis coefficientem ab temperaturis cryogenicis usque ad +500°C circiter.Nilo 36 retinet etiam bonam vim et duritiam in temperaturis cryogenicis.Applicationes includunt signa longitudinis, virgae thermostatae, partes laser et piscinae et limbus pro gasorum liquefactis et deportationibus.
Gradus relativus:
Gradus | Russia | USA | Gallia | Germania | UK |
4J32 | 32НКД 32НК-ВИ | Super-Invar Super Nilvar | Invar Superieur | - | - |
4J36 | 36Н 36Н-ВИ | Invar/Nilvar Unipsan36 | Invar Standard Fe-Ni36 | Vacodil36 Nilos36 | Invar/Nilo36 36Ni |
4J38 | - | 38NiFM Simonds38-7FM | - | - | - |
C | Ni | Si | Mn | P | S | Fe |
≤0.05 | 35.0-37.0 | ≤0.3 | 0.2-0.6 | ≤0.02 | ≤0.02 | statera |
Densitas (g/cm3) | Meltingtemperature(℃) | Facultas specifica caloris/J/(kg•℃)(20~100℃) | Electricalresistivity(μΩ·m) | Thermalconductivity/W/(m•℃) | Curie punctum(℃) |
8.10 | 1430-1450 | 515 | 0.78 | 11 | 230 |
conditio | σb/MPa | σ0.2/MPa | δ/% |
annealing | 450 | 274 | 35 |
Admisce designatio | Mediocris scelerisque expansion coefficiens / (10-6/ ) | |||||
20-50℃ | 20-100℃ | 20-200℃ | 20-300℃ | 20-400℃ | 20-500℃ | |
4J36 | 0.6 | 0.8 | 2.0 | 5.1 | 8.0 | 10.0 |
I) Scelerisque dilatatio nimis humilis inter - 250 ~ + 200 .
II) Ipsum bonum MOLLITIA et spissitudo
Invar XXXVI Application agri
● Petroleum liquefactum productio gas, repono et translationem
Screw iungo bushing inter metallum et alia materia
Duplex metallum et temperatus imperium de duplici metallo
film genus compage
umbra larva
Aviation industria CRP partes trahens mori
Framework of satellite and missilis electronic control unit infra 200 ℃
Imperium laser lens electromagneticae in tubulo vacuo auxiliari