♦Material nomen welding: Nickel Welding Wire, ErNiCrMo-4 Welding Wire, Hastelloy C276 Welding Wire
♦ MOQ: 15kg
♦ Form: MIG (15kgs/spool), TIG (5kgs/box)
♦ Size: Diameter 0.01mm-8.0mm
♦ Communia Size0.8MM / 1.0MM / 1.2MM / 1.6MM / 2.4MM / 3.2MM / 3.8MM / 4.0MM / 5.0MM
♦ signaConformat Certification AWS A5.14 ASME SFA A5.14
ErNiCrMo-4 usus est pro glutino Hastelloy C276, Nickel admixto basi et aliis materiis, Nickel admixto ferro vel ferro intemerato, etiam ad mixturam mixturae composito in chalybe adhibitam Nickel CrMo stannum. et ferro et immaculata ferro.Hoc stannum etiam adhiberi potest ad ferrum classandum cum metallo nickel-chrome-molybdaeno conglobato.Molybdenum superior contentum magnam repugnantiam praebet ut corrosio crepitationis, fovens et corrosio rima.
C | Cr | Ni | Si | Mn | P | S | Cu | Fe | V | W | Mo | Co |
≤0.02 | 14.5-16.5 | Ba | ≤0.08 | ≤1.0 | ≤0.04 | ≤0.03 | ≤0.5 | 4.0-7.0 | ≤0.35 | 3.0-4.0 | 15.0-17.0 | ≤2.5 |
Diameter | Processus | Volt | Amps | protegens Gas | |
In | mm | ||||
0.035 | 0.9 | GMAW | 26-29 | 150-190 | Transfero imbre100% Argon |
0.041 | 1.2 | GMAW | 28-32 | 180-220 | |
1/16 | 1.6 | GMAW | 29-33 | 200-250 | |
1/16 | 1.6 | GMAW | 14-18 | 90-130 | 100% Argon |
3/32 | 2.4 | GMAW | 15-20 | 120-175 | 100% Argon |
1/8 | 3.2 | GMAW | 15-20 | 150-220 | 100% Argon |
Conditio | Distrahens fortitudo MPa (ksi) | Da virtus MPa (ksi) | Prolongatio% |
AWS reauirement | 690(100) | Non certa | Non certa |
Typical eventus ut iuncta | 730 (106) | 540(79) | 39 |
MIG:75% Ar / 25% He
TIG:C% Ar
stannum resistit acido et acido vapori corrosioni. Propter altissimum molybdenum contentum, fortiter resistit ad rimas corrosionis, pituitae et cavitates corrosionis.
Late usi sunt in vase chemico tibiarum, valvularum sentinae, industriae potentiae gasorum desulfurizationis et glutino --196 applicatio 9%ni ferri.